Study Maps What Drives Wood Shrinkage Under Heat

Researchers analyzed ten wood species to identify the chemical factors behind dimensional instability during carbonization.

Updated on Nov. 13, 2026 in Chemistry

Bold flat-color editorial illustration of a wood trunk cross-section with radial cracks beside three glass vessels of pale crystals on ash.
Researchers analyzed ten wood species and found sodium and potassium lower the temperature at which wood begins to shrink during carbonization by about thirty degrees Celsius. AI Illustration. Upload story photo >

A study examining ten wood species, five softwoods and five hardwoods, has identified the factors driving dimensional instability when wood is carbonized. Monovalent alkali metal cations such as sodium and potassium lower the onset temperature of shrinkage by approximately thirty degrees Celsius.

Why it matters

Dimensional instability is a central challenge in turning wood into carbon-based materials, since uneven shrinkage can distort or crack the finished product. Identifying which wood components and metal ions control this behavior offers a basis for predicting and managing changes during processing.

The study tracked dimensional changes continuously alongside thermal degradation profiles across five softwoods and five hardwoods, with hardwoods showing greater radial shrinkage than softwoods. Its scope beyond these ten species and their chemically modified derivatives has not been established.

The details

Radial shrinkage across the wood width begins mainly as hemicellulose breaks down thermally, while longitudinal shrinkage parallel to the trunk is linked to cellulose degradation and occurs rapidly after most crystalline cellulose microfibrils have decomposed. Divalent cations such as calcium were found to stabilize the cell wall matrix and suppress excessive dimensional change.

Timeline

  1. Shrinkage anisotropy vanishes entirely once carbonization temperature surpasses 400 degrees Celsius, when the cellulose framework has broken down.

The Big Picture

The findings extend the established sequence in which hemicellulose degrades before cellulose during wood pyrolysis, linking each stage to a distinct axis of shrinkage. Earlier work treated this sequence mainly as a thermal chemistry question, whereas this study connects it directly to dimensional stability in finished carbon products.

The work points toward more predictable processing of wood-derived carbon materials, since knowing which ions and temperatures drive shrinkage can inform how wood is treated before heating. Commercial timelines for applying these findings have not been reported.

The takeaway

Treating wood with monovalent alkali metal ions can shift shrinkage to lower temperatures, so controlling the mineral content of the feedstock may help reduce distortion during carbonization.

Further reading

For related background, explore more in our Chemistry section.

Source note: This article includes information reported by Biochar Today.