Solar Encapsulant Cuts UV Power Loss in Modules
A Chinese research team reports a reactive POE film that covalently bonds a UV-absorbing additive into back-contact silicon solar modules.
Updated on Nov. 27, 2026 in Energy

Researchers from Jiangsu University of Science and Technology and Changzhou Sveck Photovoltaic New Materials developed a down-conversion POE encapsulant containing the benzotriazole derivative BTBA, published in Solar Energy. Modules using 0.6 wt% BTBA showed lower power loss than those with a physically blended additive under UV and potential-induced degradation testing.
Why it matters
Conventional UV-converting encapsulants use physically blended additives that can migrate through the polymer, potentially compromising electrical insulation and moisture barrier performance. Covalently bonding the additive into the polymer network is presented as a way to address that durability problem in solar modules.
The results come from accelerated lab tests at 85 C and 85% relative humidity on n-type monocrystalline back-contact cells in glass-glass mini-modules, with BTBA tested at 0.3, 0.6 and 0.9 wt%. Long-term outdoor durability of the encapsulant has not been reported.
The players
Jiangsu University of Science and Technology
A university in Jiangsu Province, China, that co-led the research on the reactive UV-converting encapsulant.
Changzhou Sveck Photovoltaic New Materials
A Changzhou-based materials company that co-conducted the encapsulant study with the university.
The details
The team designed BTBA with polymerizable C=C groups that form covalent bonds with the POE network during lamination, which was run at 148 C after six minutes under vacuum. The disappearance of the C=C absorption band after lamination supports the conclusion that the additive is immobilized within the film.
Timeline
Article reporting the encapsulant study published November 27, 2026.
Roadmap
Conventional blended UV-converting additives in solar encapsulants have long faced migration risks that can weaken insulation and moisture barriers. This study instead covalently bonds the additive into the POE network, a design choice aimed at extending module durability as back-contact cell technology spreads.
For solar module buyers and installers, the study suggests a path to encapsulants that lose less power under sustained UV and humidity exposure. The reported gains are from laboratory mini-modules, so field performance over years of service remains to be shown.
The takeaway
Durability claims for solar components rest heavily on accelerated test results, so readers should watch for field data before assuming laboratory gains will carry over to rooftop or utility installations.
Further reading
Explore more solar and power technology coverage in the Energy section.
Source note: This article includes information reported by pv magazine International.